| Material | 50CrMo Precision Forged Alloy Steel |
|---|---|
| Coating | American Praxair Super Hard 1342 Tungsten Cabide Powder 0.06-0.08mm |
| Width | 1850mm*340/360mm |
| Heating Treatment | Intermediate Frequency Quenching |
| Hardness | >HRC58 After Hardening |
| Material | 50CrMo Precision Forged Alloy Steel |
|---|---|
| Coating | American Praxair Super Hard 1342 Tungsten Cabide Powder 0.06-0.08mm |
| Width | 2300mm*380mm |
| Heating Treatment | Composite Heating Method |
| Hardness | >HRC58 After Hardening |
| Material | 50CrMo Precision Forged Alloy Steel |
|---|---|
| Coating | 60-80μm American Praxair Super Hard 1342 Tungsten Cabide Powder |
| Width | 2500mm×Φ385/360mm |
| Heating Treatment | Intermediate Frequency Quenching |
| Hardness | >HRC58 After Hardening |
| Packaging Details | wooden box |
|---|---|
| Delivery Time | 60~90days |
| Payment Terms | T/T |
| Supply Ability | 1000 set per year |
| Place of Origin | MADE IN CHINA |
| Material | 50CrMo Precision Forged Alloy Steel |
|---|---|
| Coating | American Praxair Super Hard 1342 Tungsten Cabide Powder |
| Coating Thickness | 60-80μm |
| Width | 1800mm*320mm |
| Heating Treatment | Intermediate Frequency Quenching |
| Material | 50CrMo Precision Forged Alloy Steel |
|---|---|
| Coating | American Praxair Super Hard 1342 Tungsten Carbide Powder 0.06-0.08mm |
| Size | 1900mm×340mm |
| Heating Treatment | Composite Heating |
| Hardness | >HRC58 After Hardening |
| Material | 50CrMo Precision Forged Alloy Steel |
|---|---|
| Coating | American Praxair Super Hard 1342 Tungsten Cabide Powder 0.06-0.08mm |
| Heating Treatment | Intermediate Frequency Quenching |
| Hardness | >HRC58 After Hardening |
| Micro Hardness | HV1250-1400 |
| Material | 50CrMo Precision Forged Alloy Steel |
|---|---|
| Coating | 60-80μm, American Praxair Super Hard 1342 Tungsten Cabide Powder |
| Width | 2200mm×Φ340mm |
| Heating Treatment | Intermediate Frequency Quenching |
| Hardness | >HRC58 After Hardening |
| Material | 50CrMo Precision Forged Alloy Steel |
|---|---|
| Coating | Tungsten Carbide Powder, 0.06-0.08mm |
| Heating Treatment | Intermediate Frequency Quenching |
| Hardness | HRC60-62 After Hardening |
| Harden Layer | 9-12mm Depth |
| Material | 50CrMo Precision Forged Alloy Steel |
|---|---|
| Coating | American Praxair Super Hard 1342 Tungsten Cabide Powder |
| Width | 2300mm×Φ380mm |
| Heating Treatment | Composite Heating Method |
| Hardness | >HRC58 After Hardening |