| Material | 45# Steel |
|---|---|
| Coating | Hard Chrome |
| Coating Thickness | 50-80μm |
| Width | 2500mm |
| Diameter | 440mm |
| Material | 50CrMo Precision Forged Alloy Steel |
|---|---|
| Coating | American Praxair Super Hard 1342 Tungsten Cabide Powder 0.06-0.08mm |
| Width | 2250mm*340mm |
| Heating Treatment | Composite Heating Method |
| Hardness | >HRC58 After Hardening |
| Material | 50CrMo Precision Forged Alloy Steel |
|---|---|
| Coating | American Praxair Super Hard 1342 Tungsten Cabide Powder 0.06-0.08mm |
| Width | 2300mm*380mm |
| Heating Treatment | Composite Heating Method |
| Hardness | >HRC58 After Hardening |
| Material | 45# Round Steel |
|---|---|
| Coating | Hard Chrome |
| Coating Thickness | 30-50μm |
| Width | 2200mm |
| Diameter | 160mm |
| Material | 45# Round Steel |
|---|---|
| Coating | Hard Chrome |
| Coating Thickness | 30-40μm |
| Width | 2300mm |
| Diameter | 160mm |
| Material | 45# Steel |
|---|---|
| Coating | Hard Chrome |
| Coating Thickness | 50-80μm |
| Width | 1900mm |
| Diameter | 340mm |
| Material | 50CrMo Precision Forged Alloy Steel |
|---|---|
| Coating | American Praxair Super Hard 1342 Tungsten Cabide Powder 60-80μm |
| Width | 2400mm×325/440mm |
| Heating Treatment | Composite Heating Method |
| Hardness | >HRC58 After Hardening |
| Material | 50CrMo Precision Forged Alloy Steel |
|---|---|
| Coating | 60-80μm Hard Chrome |
| Size | 1850mm×320mm |
| Heating Treatment | Intermediate Frequency Quenching |
| Hardness | >HRC58 After Hardening |
| Material | 50CrMo Precision Forged Alloy Steel |
|---|---|
| Coating | American Praxair Super Hard 1342 Tungsten Cabide Powder 0.06-0.08mm |
| Size | 1900mm*320mm |
| Heating Treatment | Composite Heating Method |
| Hardness | >HRC58 After Hardening |
| Material | 50CrMo Precision Forged Alloy Steel |
|---|---|
| Coating | Hard Chrome 60-80μm |
| Size | 1600mm*280mm |
| Steel Wall Thickness | ≥70mm |
| Heating Treatment | Composite Heating Method |